Degradation agent
Marine borers & salt attack
Chloride-driven fastener corrosion and, in UC5 exposure, marine organism attack.
The diagram below shows every direct connection this node has in the graph. Each line is one edge; expand a neighbour group below to read exactly why that connection exists and which standard or dataset it comes from.
Species (12)
- Norway Spruce← is vulnerable to
WI-SL resistance profile: salt = 32/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Siberian Larch← resists well
WI-SL resistance profile: salt = 70/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Western Red Cedar← moderately resists
WI-SL resistance profile: salt = 62/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Thermally Modified Ash← resists well
WI-SL resistance profile: salt = 78/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- European Oak← moderately resists
WI-SL resistance profile: salt = 66/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Acetylated Radiata Pine← resists well
WI-SL resistance profile: salt = 88/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Douglas Fir← moderately resists
WI-SL resistance profile: salt = 52/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Scots Pine (heartwood)← is vulnerable to
WI-SL resistance profile: salt = 44/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Thermally Modified Pine← resists well
WI-SL resistance profile: salt = 74/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Sweet Chestnut← moderately resists
WI-SL resistance profile: salt = 64/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Robinia (Black Locust)← resists well
WI-SL resistance profile: salt = 76/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
- Iroko (FSC certified)← resists well
WI-SL resistance profile: salt = 82/100 (ordinal, from EN 350 durability class, extractive chemistry and movement).
Source: WI-SL v1.2.0
Climate zone (2)
- Coastal Scotland← elevates risk of
Coastal Scotland has a salt load of 88/100, above the 60 threshold used here to flag a dominant degradation driver.
Source: wood.ts:climates[]
- Dubai, UAE← elevates risk of
Dubai, UAE has a salt load of 72/100, above the 60 threshold used here to flag a dominant degradation driver.
Source: wood.ts:climates[]
How edges in this graph are derivedWI-GRAPH v1.0.0
Species → agent edges come from the WI-SL resistance profile (0–100 ordinal scale derived from EN 350 durability class, extractive chemistry and movement). ≥70 is read as "resists well", 45–69 as "moderately resists", below 45 as "is vulnerable to".
Climate → agent edges fire when a climate's driver value (UV, humidity, salt or freeze-thaw load) is 60 or above, read directly from the climate dataset.
Treatment → agent / standard edges come from the paraphrased standards corpus used across the site (EN 927-1, EN 351-1, EN 350 clause 4, EN 13501-1).
Species → standard edges reuse the exact source list already published for each Global WoodIntel Score sub-score.
Machine-readable: GET /api/public/v1/graph?node=agent-marine-borers · CC BY 4.0